     Shrinkage Porosity 
 
Usually caused by Cured by
Incorrect spruing Sprues should be attached to the heaviest piece of the casting. There should be sufficient sprues to ensure the casting is adequately fed.
Flask temperature too hot. The flask temperature should be just hot enough to achieve complete fill.
 
  Casting problems
  Wax pattern problems
  Mould rubber problems