     Water Marking 

  

Usually caused by Cured by
Incorrect powder / water ratio (too much water) Using correct amount of water. (Especially important with vacuum investing machines).
Work time of investment not used up. Ensuring the work time is used up and slurry temperature is 20- 22oC.
 
  Casting problems
  Wax pattern problems
  Mould rubber problems
Mixing guide
De-wax and  burnout cycles